Jump to content
SAU Community

Recommended Posts

The only thing you have proven is that the particular coating that you tested was not effective, not ceramic coating in general.

If a ceramic coating is only rated to 500oC and your gas flow has a temp of 800oC then obviously you wont see any difference. Try a coating thats rated to 3000oC.... then you will see a difference, even if you apply it to half your manifold.

Checkout some results at http://www.carcraft.com/techarticles/80038

Enjoy

Thanks, I enjoyed that immensely.

:laughing-smiley-014: :laughing-smiley-014: :laughing-smiley-014: :laughing-smiley-014:

Infact I believe the expression is ROFLMAO or similar.

Have a search for infra red thermometers. Look at the instructions. You will find that they DO NOT work on anything other than matt black surfaces...

The coating was sold as heat insulation. Good insulators do not change their coefficient of thermal conductivity much with changes in temperature.

My contention is that the coating is not effective, not because of anyshortcomings in the characteristics of the ceramic, but simply that the applied thicknesses are insufficient to create any meaningful resistance to the conductivity of the pipe.

  • Replies 50
  • Created
  • Last Reply

Top Posters In This Topic

Top Posters In This Topic

Posted Images

You are saying that ALL ceramic coatings are useless because of the results of ONE test on ONE product at ONE thickness?

Well, geeeee, you've convinced me ... NOT.

What I am saying is that in the thickness typically applied the product does not demonstrate any sustantial heat insulating properties. I have explained the photo & reasons for my opinion.

However, in light of your eloquent reply I am at a loss to further explain anything. :w00t:

I just have a few issues with what you are saying:

1) you applied the coating to the inside of the manifold, but only half of it and along the direction of flow of the gas? Thermal transfer occurs between the gas and the uncoated segment of pipe and then directly up the pipe to what was once a cooler section so that the temperature converges to an equilibrium along the surface.

2) Im talking about coating the outside of the manifold.

3) Not all "ceramic coatings" are homogenous, some are layers of different heat resistent matrial and anti-oxidsing properties.

4) what's a typical thickness? I can only infer that you are limited by the thickness of the coat on the inside of the manifold as any gains from insulation may be negated by a reduction in cross sectional area of the pipe.

djr81, I do appreciate your feedback :w00t:

1) you applied the coating to the inside of the manifold, but only half of it and along the direction of flow of the gas? Thermal transfer occurs between the gas and the uncoated segment of pipe and then directly up the pipe to what was once a cooler section so that the temperature converges to an equilibrium along the surface.

Coating was applied to the turbo dump pipe. Unsure what you mean about the direction of flow of the gas (right to left if that is what you are wondering) Have a look at the temperature of the flange metal. It is below the temperature of the RHS of the pipe, ie the dump pipe. Makes what you are saying impossible.

4) what's a typical thickness? I can only infer that you are limited by the thickness of the coat on the inside of the manifold as any gains from insulation may be negated by a reduction in cross sectional area of the pipe.

WARNING: Science content (oh shit)

For a two layered ie coating + metal system the steady state one dimensional heat equation looks like this:

Q =

(T0 - T2)

----------------------------

(delta X1/(k1A)) + (delta X2/k2A))

Where:

Q = heat flow

T0 is the internal temperature

T2 is the external temperature

Delta x1 & delta x2 is the thickness of the metal and the ceramic.

k1 is the thermal conductivity of the internal metal and/or coating (whichever way around you arrange it, measured in W/mK

k2 is the thermal conductivity of the external metal and/or coating (whichever way around you arrange it, measured in W/mK

A is the surface area.

For the anoraks this is simply an externion of Fourier's law.

Salient points are:

Doesn't matter if the coating is internal or external.

For an individual layer the two fundamentally important variables are the k value, ie the thermal conductivity of the material & the thickness of the layer delta X.

This is why I have made the point that with the thicknesses typically applied, the coating doesn't have any real chance of insulating the pipe. My old textbook (Janna) puts asbestos at 0.113W/mK and glass fibre at 0.035 which are two of the best insulators, although you can't use asbestos anymore for good reasons.

To anyone using the heat wrap tape, please note the following:

DON"T BREATH IT IN, PARTICULARLY AFTER IT HAS BEEN HEATED.

You have been warned.

Edited by djr81

interesting discussion guys but I'm convinced that the coating is a good thing. i intend to get GTR turbine housings, exh manifolds and stainless long-style Trust dumps coated. The thing I'm not sure about is what temp coating to go for. HPC have a low 800C and a high 1200C temp coating plus a variation to increase the temp resistance of the 800C coating. the 1200C coating is around 3 times the price of the 1200C coating, what do you recommend in terms of what to coat in what?

cheers

djr81 I'm still not convinced that you would really see any surface temperature difference on such a short length of pipe, only half coated where conductivity occurs back up the pipe through the metal. Perhaps initially you would but after running for some time I doubt it. The reason the flange is different is probably due to a non-metallic gasket or possible slightly different metal ( and hence difference thermal conductivity + thickness).

However, I definately agree that the thickness and conductivity are the determining factors [ as can be inferred from the equations ]. Also, dont forget that there are other factors involved that effect the distribution of heat, turbulance + edge effects, etc.

One should be able to deduce mathematically the required thickness of ceramic to achieve a 30% reduction in Q [ and hence T].

Cheers

I thought this thread was pretty clear?

Dont bother with ceramic coating, buy some thermal wrapping and steel cable ties and thats the best way about it?

So... lets not even bother considering ceramic coating. I mean, whats the benefit over wrapping?

From my experiance, wrapping drops surface temps HEAPS. Enough to be able to tough for a second without burning your fingers off.

I thought this thread was pretty clear?

Dont bother with ceramic coating, buy some thermal wrapping and steel cable ties and thats the best way about it?

So... lets not even bother considering ceramic coating. I mean, whats the benefit over wrapping?

From my experiance, wrapping drops surface temps HEAPS. Enough to be able to tough for a second without burning your fingers off.

Good luck wrapping your engine block or head ;0

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now



  • Similar Content

  • Latest Posts

    • After using a protractor for an actually accurate assessment of what is required,  and by NOT using my uncalibrated eyeball I worked out I need a 25° silicone bend from the TB ro the MAF, but, my choice was either a 30° or a 23° (23° is a weird spec), so I grabbed the 23° one from Raceworks I also grabbed 1mtr of 3" straight from Just Jap, I needed 350mm, but they only had 300mm, or 1mtr lengths....meh Also ordered a 1/2" hose bulkhead fitting from fleabay, this has a smoothish mushroom looking head (they are designed for below the water line of boats) that will fit inside the bend, the hose bit and threaded bit looks to long, but nothing that a hacksaw cannot fix if required, the hose will then just get jamed on the threaded bit up to the retaining nut Fingers crossed and the unsightly amount of hose clamps will be reduced down to 4 once all the parts arrive 
    • Oil change does not trigger code 21. Code 21 is for coilpacks primary side connection. You can try to clear the code with a battery disconnect, hold down the brake pedal to drain capacitors through the brake lights with the ignition on for 10-15 seconds before you reconnect the battery. I have seen R35 coil conversion permanently cause this code with no ill effects so it might be the resistance it wants to see isn't quite right on one or more coilpacks. Could be inside the ECU, could be the harness, could be a coil. You can test it all if you want or just ignore until the car actually starts misfiring.
    • I forgot you have a Nistune ECU. Use Nistune to do all the tests I mentioned instead of faffing with 30+ year old electrical connectors. You can read MAF volts off that too, there are reference values in the service manual to tell you roughly what it should be in different conditions.
    • No. I think it might be the AFM. Hence the use of the terms "swaptronics", which implies the use of swapping out electronics for the purpose of diagnosis. It's about the only way to prove that a small/niggling/whatever problem with an AFM or a CAS or similar is actually caused by that AFM/CAS/whatever. A known good item swapped in that still gives the same problem is likely to be caused somewhere else. They're all the same. Spraying AFMs with cleaner is an each way bet between cleaning it and f**king it.
    • Oh wow! This might actually work amazingly. Do you know the ratio of the diff? I was told the only thing you need to make sure of is if the front & rear diff ratios are the same. Ours is a 4.083 Thanks!
×
×
  • Create New...