Jump to content
SAU Community

Recommended Posts

Hi guys,

I just finished my first real alloy fabrication project.

I bought a TIG about 2 months ago for some weekend fun :)

Decided to make a catch can/washer bottle for my R33 out of 2mm alloy sheet.

I'm still trying to get the hand and feed speed right, but hopefully more seat time will help!

Any tips or criticism would be greatly appreciated!

Chris :)

post-55684-13964117687792_thumb.jpgpost-55684-13964117897538_thumb.jpgpost-55684-13964118094256_thumb.jpg

Link to comment
https://www.sau.com.au/forums/topic/441396-first-attempt-at-alloy-fabrication/
Share on other sites

Looks pretty good to me. Better than some workshops. :)

Practice is the only way to get better. Were you using a foot pedal? I gotta get me one, stopping to turn the dial down as the work heats up is a pita.

The cap was an eBay job- cost $28 including postage which i thought was reasonable.

I am just using the T2 control on the torch at the moment but would like to get a pedal in the future.

My biggest challenge is training my left-hand to feed properly!

Looks good, try stepping up to 3mm for items like these, makes life a hell of alot easier and you dont need to worry about a foot pedal for the tig, I'm a boily by trade who does way to much tig and i f**king hate foot pedals. If you're having lots of problems with heat soaking the material my advice is to Tack it how you want, than put a solid tack on each outside corner were the 3 pieces of material come together than its simple a case of welding from one tack to the other and blowing the material offf with an air gun inbetween runs aswell as dropping the amperage a a touch after the first few. If you feel its getting to hot Let it sit there for 10-15 minutes inbetween runs.. Take your time and be patient.

  • Like 1

Getting there bud, tonal it easier to get even ripples, get the use the move, stop, add technique makes it a lot easier to get the " stack of dimes" beads as both hands don't have to work at the same time with bigger runs I make tacks in the corners then 4 inches apart with no filler so it doesn't ruin the run you are about to do and clean surfaces and good fit is key, have fun mate

  • 3 weeks later...

Nah wasn't me it was probably a bloke called David lol.

My car is off the road at the moment getting a new turbo upgrade so hopefully will be out and about again soon. One of your catch cans would finish it off nicely I reckon ;)

  • 2 weeks later...

Nah wasn't me it was probably a bloke called David lol.

My car is off the road at the moment getting a new turbo upgrade so hopefully will be out and about again soon. One of your catch cans would finish it off nicely I reckon ;)

If you're serious about a catch can PM me, I've just moved up to darwin and have a little bit of time to do small fab jobs. Also check my thread in the fabrication section if you want to see previous work i've done.

For anyone who is interested I have another one which is almost finished.

Don't have any idea what they are worth to sell but Ill post a picture of the finished item and if someone wants to make an offer on it, go for it!

Cheers

Chris

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now


  • Similar Content

  • Latest Posts

    • Which is why I didn't mention that hardness testing, and specifically mentioned the bore and deck thickness testing. Yeah, not really. The bore temperature will be a lot more even around the top half inch or so, where the material distribution is dominated by the deck, and which is the only place where the bore surface temperature heating any gas in the cylinder is likely to have any effect on detonation. Think about it. Another inch or so down the bore, you might have a hotter spot. The gas there might get a bit hotter, then the piston rises squeezes that gas away from there at high speed and mixes it with other gas from nearby. Instant dilution of the problem. I'd be surprised if it was an issue at any time other than in racing engines or OEM dev engines being run at the ragged edge of tuning. Say what now?
    • https://dsportmag.com/the-tech/education/engine-tech-material-hardness-testing/ The PRP testing on block hardness I'm not sure how much it actually can be trusted. The thinner cylinder walls on RBs is a bit of a problem vs 2JZ but it really depends on the design goal. Siamesed cylinder bores like a 2JZ cause uneven cylinder wall temps too, which means a bit of distortion induced by that + the hotspot can affect knock margin. Something that actually gives me a bit of pause with the PRP block, whether super thick cylinder walls are going to keep it from being drop-in compatible on an otherwise OEM rebuild. 
    • Yeah very valid point. I am waiting for one of the other tuners to come back from vacation so he can help me a bit when the cat is installed again. In the meantime I am going to finish up my polishing and ceramic coating that I have started myself.    N45 Dr Beasley product is highly recommended for a paint primer / polisher. Using this EXO Gtechniq also for the ceramic but next time might use the light serum before hand also. Looks great. 
    • Running rich in conditions where it shouldn't probably won't do great things for catalytic converter lifespan. I would fix that sooner than later.
    • Yes, important point. Watch the Motive videos with Herman thickness testing the bores and deck. You do not want to push the unlucky (thin) block as hard as you can push the average block.
×
×